Stress Corrosion Cracking of Nickel Based Alloys in Water-Cooled Nuclear Reactors: The Coriou Effect presents the latest information on brittle failure of metals in corrosive chemical environments under the influence of tensile stresses.Nickel alloys are more resistant to SCC as well as high temperatures and have been widely used in more challenging environments such as nuclear power plants. Howev...
Read more
E-book
epub
Price
135.00 £ * Old Price 162.00 £
Stress Corrosion Cracking of Nickel Based Alloys in Water-Cooled Nuclear Reactors: The Coriou Effect presents the latest information on brittle failure of metals in corrosive chemical environments under the influence of tensile stresses.Nickel alloys are more resistant to SCC as well as high temperatures and have been widely used in more challenging environments such as nuclear power plants. Howev...